Particles velocity speed – Ultrasound (over 1200 m/s)
Coating porosity – 0.5%
Deposited Materials
– Metals and alloys
– Ceramics – Al2O3
– Composites – WC/Co
– Combinations of above
Please see the table below for a list of sample processes.
WC-based coatings with hardness of up to 1300 HV300
Al2O3-based coatings with hardness of up to 1300 HV300
Ti-based coatings with hardness of up to 1000 HV300
Coating porosity typically below 0.5%
Low compressive residual stresses in coatings
Negligible oxide content in coatings